Gh3039 High Strength Corrosion Resistant Nickel-Based Superalloy For Demanding High-Temperature Applications

Contact Supplier
Product Details
Brand Name: Zhonggong Special Metallurgy
Model Number: GH3039 alloy
Place of Origin: China
Price: Price is negotiated based on the required specifications and quantity
Payment Terms: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability: 5000 tons per month
Delivery Time: 5-8 working days, depending on the parameters required for negotiation
Packaging Details: Standard export packaging, or packaging as required
Minimum Order: 100KG
Certification: ISO Certificate
Composition: Nickel-based superalloy containing Chromium, Cobalt, Iron, and other elements
Density: 8.23 g/cm³
Melting Point: 1320-1370°C (2408-2498°F)
Tensile Strength: 850-1100 MPa (at room temperature)
Yield Strength (0.2% offset): 450-700 MPa
Elongation: 30-50%
Thermal Conductivity: 9.8 W/m·K (at 100°C)
Specific Heat Capacity: Specific Heat Capacity
Coefficient of Thermal Expansion: 13.6 µm/m·K (20-100°C)
Electrical Resistivity: 1.10 µΩ·m (at 20°C)
Magnetic Properties: Non-magnetic
Description
GH3039 alloy, a high-performance nickel-based superalloy, excels in demanding environments due to its exceptional mechanical strength, oxidation ...